In vitro and vivo biocompatibility and degradability of low-alloyed Mg-Zn-Ca-MgO composite as bone repair biomaterials

ผู้แต่ง

  • Shuquan ZHANG Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Jiangtao FENG Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Chaokun TANG School of Materials Science and Engineering, Tianjin University of Technology, Tianjin, 300384, China
  • Ran PANG Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Xinglong ZHANG Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Chenguang LI Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Weihao ZHANG Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Fengxin ZHOU Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Feng XUE Department of Orthopedics, Integrated Chinese and Western Medicine Hospital, Tianjin University, Tianjin, 300072, China; Department of Orthopedics, Tianjin Hospital of Integrated Chinese and Western Medicine, Tianjin, 300100, China; Department of Orthopedics, Tianjin NanKai Hospital, Tianjin, 300100, China
  • Shaoyuan LYU School of Materials Science and Engineering, Tianjin University of Technology, Tianjin, 300384, China
  • Minfang CHEN School of Materials Science and Engineering, Tianjin University of Technology, Tianjin, 300384, China; National Demonstration Center for Experimental Function Materials Education, Tianjin, 300384, China; Key Laboratory of Display Materials and Photoelectric Device (Ministry of Education), Tianjin, 300384, China
  • Hao WANG Medical School of Tianjin University, Tianjin University, Tianjin, 300072, China

DOI:

https://doi.org/10.55713/jmmm.v34i1.1910

คำสำคัญ:

magnesium alloy, Corrosion, Bone regeneration, Cell-compatibility

บทคัดย่อ

Abstract

Magnesium alloys have gained attention as biodegradable bone repair biomaterials. Unlike non-biodegradable materials like titanium and tantalum, biodegradable implants offer advantages in promoting bone healing and minimizing chronic inflammatory reactions. However, the impact of the implant's degradation on the osteogenic environment remains a concern. The Mg-Zn-Ca-MgO composite, being biocompatible and containing osteogenic ions, is a promising candidate. This study assesses the degradability and in vitro/in vivo biocompatibility of two Mg-Zn-Ca-MgO composites with varying degradation rates. The Mg-1Zn-0.2Ca-1.0MgO composite was prepared, and leaching solutions were created following standard protocols. MC3T3-E1 cell cultures were conducted to assess cell toxicity, alkaline phosphatase (ALP) staining, cytoskeleton morphology, and osteogenic protein expression. In vivo biodegradation and bone regeneration capacity were evaluated in rat femoral condyles. Benefiting from the more protective corrosion product layer on the surface, the ultra-fine grained (UFG) composite showed better corrosion resistance and lower Mg2+ release than the coarse-grained (CG) composite. UFG material exhibited higher cell viability, cytoskeleton integrity, ALP secretion, and osteogenic protein expression. In vivo, UFG composites led to greater bone regeneration and exhibited excellent biocompatibility. The UFG Mg-Zn-Ca-MgO composite demonstrates enhanced biocompatibility, corrosion resistance, and bone regeneration potential. This study highlights the importance of controlling Mg ion release for optimal bone healing in biodegradable materials.

Downloads

Download data is not yet available.

เอกสารอ้างอิง

M. P. Staiger, A. M. Pietak, J. Huadmai, and G. Dias, "Magnesium and its alloys as orthopedic biomaterials: a review," Biomaterials, vol. 27, no. 9, pp. 1728-1734, 2006.

N. Singh, U. Batra, K. Kumar, N. Ahuja, and A. Mahapatro, "Progress in bioactive surface coatings on biodegradable Mg alloys: A critical review towards clinical translation," Bioact Mater, vol. 19, pp. 717-757, 2023.

Y. Chen, Z. Xu, C. Smith, and J. Sankar, "Recent advances on the development of magnesium alloys for biodegradable implants," Acta Biomater, vol. 10, no. 11, pp. 4561-4573, 2014.

S. Y. N. Wang, H. Shi, Y. Song, H. Sun, Q. Wang, L. Tan, and S. Guo, "Magnesium alloys for orthopedic applications: A review on the mechanisms driving bone healing," Journal of Magnesium and Alloys, vol. 10, no. 12, pp. 3327-3353, 2022.

Y. H. Chang, C. C. Tseng, C. Y. Chao, C. H. Chen, S. Y. Lin, and J. K. Du, "Mg-Zn-Ca alloys for hemostasis clips for vessel ligation: In Vitro and In Vivo studies of their degradation and response," Materials (Basel), vol. 13, no. 13, 2020.

F. Feyerabend, F. Witte, M. Kammal, and R. Willumeit, "Unphysiologically high magnesium concentrations support chondrocyte proliferation and redifferentiation," Tissue engineering, vol. 12, no. 12, pp. 3545-3556, 2006.

Z. Y. Fan, Y. B. Zuo, and B. Jiang, "A new technology for treating liquid metals with intensive melt shearing," Materials Science Forum, vol. 690, pp. 141-144, 2011.

M. D. S. Thanka Rajan, A. Arockiarajan, "In vitro assessment of corrosion resistance and biocompatibility of tantalum-niobium oxide surface-functionalized Mg alloy," Materials Chemistry and Physics, vol. 301, p. 127560, 2023.

D. Zhao, K. Yu, T. Sun, X. Jing, Y. Wan, K. Chem, H. Gao, Y. Wang, L. Chen, X. Guo, and Q. Wei, "Material–Structure–Function integrated additive manufacturing of degradable metallic bone implants for load-bearing applications," Advanced Functional Materials, vol. 33, no. 16, p. 2213128, 2023.

Y. Wang, Y. Fan, and H. Liu, "Macrophage polarization in response to biomaterials for vascularization," Annals of Biomedical Engineering, vol. 49, no. 9, pp. 1992-2005, 2021.

M. Wang, Y. Yu, K. Dai, Z. Ma, Y. Liu, J. Wang, and C. Liu, "Improved osteogenesis and angiogenesis of magnesium-doped calcium phosphate cement via macrophage immunomodulation," Biomaterials Science, vol. 4, no. 11, pp. 1574-1583, 2016.

ดาวน์โหลด

เผยแพร่แล้ว

2024-02-05

วิธีการอ้างอิง

[1]
S. ZHANG, “In vitro and vivo biocompatibility and degradability of low-alloyed Mg-Zn-Ca-MgO composite as bone repair biomaterials”, J Met Mater Miner, ปี 34, ฉบับที่ 1, น. 1910, ก.พ. 2024.

ฉบับ

บท

Original Research Articles